Supreme 3HT

One component, toughened epoxy adhesive, sealant and coating
Key Features
  • Fast curing
  • Superior toughness
  • Holds up well to thermal cycling
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
100,000-200,000 cps
Cure Schedule
250°F for 20-30 minutes, 300°F for 5-10 minutes
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +350°F
Dielectric Constant
3.9
Tensile Lap Shear Strength
1,600-1,800 psi
תמונה
Supreme 3HT One Part Epoxy System
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Packaging
Product Description

Master Bond Supreme 3HT blends together superior toughness, easy processing and exceptional physical strength properties, along with very good thermal cycling capabilities. It is easy to use as it requires no mixing; simply heating to 250-300°F for a short period of time as noted below is required. Essentially, its working life is unlimited because it will not cure until it is heated to the required temperature. Supreme 3HT has low shrinkage upon curing as well.

Supreme 3HT is a fine adhesive; it bonds well to a wide variety of substrates including metals, composites, ceramics, glass as well as many plastics and rubber materials. Its excellent toughness imparts a superior capacity to resist thermal cycling and shocks. The combination of these properties enables Supreme 3HT to be particularly effective for bonding dissimilar substrates. It is a highly reliable electrical insulator and has very good resistance to chemicals including water, oils and fuels. Its service temperature is a robust -100°F to +350°F. It is 100% reactive and does not contain any diluents or solvents. The natural color of Supreme 3HT is brown to tan but other colors are also available. This epoxy is very useful in aerospace, electronic, electrical, optical and specialty OEM applications where the operating conditions demand high performance, easy handling and fast curing.

Product Advantages

  • One component system; no mixing required, fast curing, minimum cure temperature of 250°F
  • Unlimited working life. Will not cure at room temperature
  • Less rigid than “typical” epoxies
  • Bonds well to a wide variety of substrates
  • Superior capability to withstand thermal cycling and shocks
  • Outstanding physical strength profile
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.