Supreme 45HTQ

Two component epoxy system for bonding, sealing and casting
Key Features
  • Outstanding temperature and chemical resistance
  • High compressive strength
  • Withstands abrasive forces
  • Widely used in oil and gas processing
Typical Properties
Viscosity
20,000-30,000 cps
Cure Schedule
4 to 6 hours at 250°F, 4 to 5 hours at 350°F, optimal cure schedule is 300°F for 2 hours, followed by post curing at 350°F for 4 to 6 hours.
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Tensile Lap Shear Strength
2,100-2,300 psi
Tensile Modulus
500,000-550,000 psi
תמונה
Supreme 45HTQ Two Part Epoxy Compound
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Product Description

Master Bond Supreme 45HTQ is a two component, toughened, quartz filled epoxy for high performance bonding, sealing and casting. Its mix ratio is a forgiving 100 to 30 by weight and the working life after mixing is 12-24 hours. It is a moderate viscosity system. The system requires oven curing with several options. The first is 4 to 6 hours at 250°F, whereas another is 4 to 5 hours at 350°F. The optimal cure schedule is 300°F for 2 hours, followed by post curing at 350°F for 4 to 6 hours. It is 100% reactive and does not contain any solvents or diluents.

First and foremost, Supreme 45HTQ has excellent resistance to acids, bases and solvents. It bonds well to a wide variety of substrates, including metals, composites, ceramics and many different plastics. After curing, it has a number of desirable physical strength properties including high modulus and exceptional compressive strength. It is a toughened system that can withstand rigorous thermal cycling. An important part of this formulation is its quartz filler. This lends to its increased dimensional stability and greater abrasion resistance. Supreme 45HTQ is a reliable electrical insulator. The service temperature range is from -60°F to +450°F. The color of Part A is tan and Part B is brown. When these properties are combined, it allows Supreme 45HTQ to be used as a “go to” epoxy for downhole applications as well as other situations where the properties mentioned previously are required.

Product Advantages

  • Exceptionally long pot life at room temperature
  • Resists chemicals, especially those encountered downhole
  • Withstands elevated temperatures
  • Extraordinary compressive strength
  • Holds up well against abrasive forces
  • Passes 1,000 hours of 85°C/85% RH
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.