UV10TK40M

One component, higher viscosity UV curable system for bonding, sealing and coating
Key Features
  • Outstanding optical clarity
  • High glass transition temperature
  • Passes NASA low outgassing specifications
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
30,000-60,000 cps
Cure Schedule
cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with 20-40 milliwatts per cm²
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +450°F
Glass Transition Temperature (Tg)
135-140°C
Refractive Index
1.55
תמונה
One component, high viscosity UV curable system UV10TK40M
Certifications

1,000 Hours at 85°C/85% RH

Meets EU Directive 2015/863

ASTM E595 Compliant

Product Description

Master Bond UV10TK40M is a higher viscosity, one part UV system for bonding, sealing and coating with good optical clarity, excellent physical properties and a high glass transition temperature (Tg) of 135-140°C. UV10TK40M cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with 20-40 milliwatts per cm². The rate of cure depends upon the distance from the light source, the thickness of the section and the intensity of the light source. The system can cure in sections up to 1/4 inch thick. However, when bonding, sections of a few thousandths of an inch are more than adequate. Master Bond UV10TK40M is not oxygen inhibited and therefore does not require any special treatment in that regard. It bonds well to glass, surface treated metals and plastics such as polycarbonates and acrylics, among others. Its chemical resistance is particularly good as it resists water, oils, acids, bases and solvents well. It is also an effective sealing and coating material. The system does not contain any solvents or diluents and none are released during cure. UV10TK40M combines low shrinkage with exceptional dimensional stability. UV10TK40M is an outstanding electrical insulator with a temperature range of -60°F to +450°F. It is effectively used for high production applications where fast fixture times and rapid curing are critical. UV10TK40M is best used in fiber-optic, optical, opto-electronic and electronic industries where high temperature resistance and higher viscosity are needed.

Product Advantages

  • One component system
  • No oxygen inhibition
  • Reliable electrical insulator
  • Adheres well to many substrates
  • Outstanding optical clarity; excellent light transmission
  • Meets NASA low outgassing specifications
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.