X-5

Highlight

High Performance, Elastomer-Based, One-Component Adhesive for Fast & Durable Bonding and Sealing

Typical Properties
Viscosity
3000 cps
Service Temperature Range
-75 to 275°F
Specific Gravity
0.91
Volume Resistivity
>10¹⁰ ohm-cm
תמונה
Elastomer Based, One Component Adhesive
Applications
Product Description

Master Bond X-5 is a specially formulated, synthetic, elastomer-based, one component adhesive for high performance bonding and sealing. This adhesive bonds well in both shear and peel to similar and dissimilar surfaces including metals, woods, most plastics, ceramics, glass, rubber, paper, leather, wallboard, insulation, concrete, plastic foams and stone. Master Bond X-5 contains 30% solids and has a carefully designed solvent blend which evaporates as the cure proceeds. An initial set takes place in Master Bond X-5 as soon as most of the solvent has evaporated. The strength of this initial set usually suffices to maintain the assembly and, with some adherents, will exceed the strength of the material. Bond strength increases as evaporation of the solvent progresses, reaching a maximum when all of the solvent has been removed. Master Bond X-5 adhesive has a solids content of 30% by weight as supplied.

All surfaces should be carefully cleaned and dried before application. They should be free of grease, oil, dirt and other contaminants for optimal results. Conventional cleaning methods such as solvent washing, vapor degreasing, etching, etc. are applicable. A convenient way of determining when thorough cleaning has been accomplished is to flow water over a vertically held coated surface. If the water runs off in a continuous film, cleaning is satisfactory.

Master Bond X-5 is a readily flowable liquid. It can be further thinned with ketone solvents to reduce viscosity. Cured Master Bond X-5 adhesive retains its high strength even after exposure or immersion in water and in many other chemicals including fuels, oils, etc. Master Bond X-5 also features superior electrical insulation properties.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.