EP62-1LO

High temperature resistant, NASA low outgassing epoxy compound
Key Features
  • Convenient handling, long working life
  • Cures rapidly at moderate temperatures
  • Superior bond strength properties
  • Widely used for its chemical resistance
Typical Properties
Viscosity
4,000-8,000 cps
Cure Schedule
4-6 hours at 60-70°C, 20-40 minutes at 80-100°C or 10 minutes at 125°C
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.2
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
EP62-1LO Two Part Epoxy
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Product Description

Master Bond EP62-1LO is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a very forgiving 100 to 10 mix ratio by weight. The pot life of 100 grams is greater than 12 hours. Typical cure schedules range from 4-6 hours at 60-70°C, 20-40 minutes at 80-100°C or 10 minutes at 125°C. The cured epoxy resin exhibits remarkably high thermal stability with a glass transition temperature of 140-145°C. Also noteworthy is its outstanding chemical resistance to acids, bases, many solvents and other chemicals, even at elevated temperatures. This system has excellent electrical insulation properties. The color of Part A is clear and Part B is dark brown. EP62-1LO is primarily used as an adhesive, sealant and coating where the epoxy will be exposed to very aggressive conditions as well as where a long open time and NASA low outgassing are required.

Product Advantages

  • Easy to use, very forgiving 100 to 10 mix ratio by weight (will fully cure using 100 to 5 mix ratio)
  • Superior resistance to a wide variety of chemicals, even at high temperatures
  • Service temperature range of -60°F to +450°F
  • Versatile cure schedules at various elevated temperatures
  • Excellent physical strength properties
  • Meets NASA low outgassing standards
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.