High temperature resistant, NASA low outgassing epoxy compound

Key Features

  • Convenient handling, long working life
  • Cures rapidly at moderate temperatures
  • Superior bond strength properties
  • Widely used for its chemical resistance

Product Description

Master Bond EP62-1LO is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a very forgiving 100 to 10 mix ratio by weight. The pot life of 100 grams is greater than 12 hours. Typical cure schedules range from 4-6 hours at 60-70°C, 20-40 minutes at 80-100°C or 10 minutes at 125°C. The cured epoxy resin exhibits remarkably high thermal stability with a glass transition temperature of 140-145°C. Also noteworthy is its outstanding chemical resistance to acids, bases, many solvents and other chemicals, even at elevated temperatures. This system has excellent electrical insulation properties. The color of Part A is clear and Part B is dark brown. EP62-1LO is primarily used as an adhesive, sealant and coating where the epoxy will be exposed to very aggressive conditions as well as where a long open time and NASA low outgassing are required.

Product Advantages

  • Easy to use, very forgiving 100 to 10 mix ratio by weight (will fully cure using 100 to 5 mix ratio)
  • Superior resistance to a wide variety of chemicals, even at high temperatures
  • Service temperature range of -60°F to +450°F
  • Versatile cure schedules at various elevated temperatures
  • Excellent physical strength properties
  • Meets NASA low outgassing standards

Industrial Certifications


ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging


Cans

Double Barrel Cartridge

FlexiPak®

Gun Applicator

Pails

Syringes

EP62-1LO is available is various sizes and units to accommodate customer's needs.