EP110F8-1

Two component, high performance epoxy for potting, sealing, encapsulating and casting
Key Features
  • Exceptionally long working life at room temperature
  • Low viscosity
  • Outstanding electrical insulation properties
  • Highly resistant to thermal cycling and shock
Typical Properties
Viscosity
2,500-5,000 cps
Cure Schedule
4-6 hours at 250-300°F
Hardness
65-75 Shore D
Service Temperature Range
-80°F to +325°F
Dielectric Constant
2.81
Elongation
85-95%
תמונה
EP110F8-1 Two Part Epoxy
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP110F8-1 is a two component high performance epoxy resin system with a long pot life (at least 2-3 days at room temperature). It is used primarily for potting, sealing, encapsulating and casting. This low viscosity system has a convenient and very forgiving one to two mix ratio by weight. It requires an elevated temperature cure at 250-300°F. A typical cure schedule would be 4-6 hours at 250-300°F. For optimum properties, a post cure of 3-5 hours at 350°F is recommended. It should be noted that even without the optional post cure, EP110F8-1 will perform very well. EP110F8-1 has no solvents or diluents and has low shrinkage upon cure.

It adheres well to a wide variety of substrates, including metals, composites, glass and many plastics. At the forefront of its property profile are superior electrical insulation properties. Also, its physical strength properties of moderate tensile strength, lower modulus and high elongation, translates into its ability to withstand severe thermal cycling and shock. It resists water, oils, fuels and a number of acids and bases quite well. The color of Part A is clear while the color of Part B is amber. The service temperature range is -80°F to +325°F. It can be used in applications where high performance electrical insulation properties and resistance to thermal cycling are required.

Product Advantages

  • Lower viscosity liquid; good flowability
  • Long working life at room temperature
  • Outstanding thermal shock resistance
  • Superior toughness over a wide temperature range
  • Top tier electrical insulation properties
  • Good mechanical strength properties
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.