EP72M4

Two component, flexibilized epoxy for bonding, sealing, and coating
Key Features
  • Convenient handling and processing
  • Room temperature curable
  • Withstands rigorous thermal cycling and shock
  • Good shear and peel strength


Note: EP72M4 complies with RoHS3 Directive (EU) 2015/863. It is a new version of EP72M3, which has been discontinued.

Typical Properties
Viscosity
paste
Cure Schedule
75°F in 3-5 days; overnight at 75°F followed by 3-4 hours at 135-150°F
Hardness
30-40 Shore D
Service Temperature Range
-100°F to +250°F
Dielectric Constant
3.9
Tensile Modulus
50,000-100,000 psi
תמונה
Two component, highly flexible epoxy system EP72M4
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond polymer adhesive EP72M4 is a two component, highly flexible epoxy system for bonding, sealing, and coating. This high viscosity system has a very user friendly one to one mix ratio by weight or volume with an exceptionally long open time of 5-7 hours. EP72M4 will cure at room temperature in 3-5 days. An alternative curing schedule is overnight at room temperature followed by 3-4 hours at 135-150°F. EP72M4 does not contain any solvents or diluents and has very low shrinkage upon curing.

EP72M4 bonds well to a wide variety of substrates including metals, glass, composites, rubbers, and many plastics. It features high bond strength in both peel and shear modes. Since it is a flexible system it is particularly well suited for bonding dissimilar substrates. It withstands rigorous thermal cycling as well as thermal and mechanical shocks. EP72M4 has good resistance to water, oils and fuels. It is a reliable electrical insulator.

The standard color of Part A is translucent and Part B is amber, although other colors are available. A non-drip version called EP72M4ND is also available. Master Bond EP72M4 is most likely to be used in aerospace, electronic, optical and specialty OEM applications when a highly flexible, high viscosity epoxy with the set of properties mentioned above is beneficial.

Product Advantages

  • Non-critical one to one mix ratio by weight or volume
  • High viscosity but spreads evenly and smoothly
  • Very long open time
  • Many cure schedule options
  • Outstanding toughness and flexibility
  • A good fit for bonding dissimilar substrates
  • Fully complies with RoHS and REACH regulations
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.