EP42HT-4AOMed Black

Two part, thermally conductive epoxy for medical device manufacturing
Key Features
  • Exceptional heat resistance
  • Thermally conductive and electrically insulative
  • Cryogenically serviceable
  • Passes ISO 10993-5 and USP Class VI
Typical Properties
Viscosity
Part A: 50,000-120,000 cps, Part B: 200-1,000 cps
Cure Schedule
overnight at 75°F, followed by 2-3 hours at 150-200°F
Hardness
85-90 Shore D
Service Temperature Range
4K to +400°F
Coefficient of Thermal Expansion
18-21 x 10⁻⁶ in/in/°C
Tensile Modulus
500,000-550,000 psi
תמונה
EP42HT-4AOMed Black Two Component Epoxy
Certifications

Meets EU Directive 2015/863

USP Class VI Medical

ISO 10993-5 for Cytotoxicity

1,000 Hours at 85°C/85% RH

Packaging
Product Description

Master Bond EP42HT-4AOMed Black is a two component epoxy adhesive, sealant, coating and casting system with a number of noteworthy features. It has a forgiving mix ratio of 100 to 40 by weight along with very good flow properties. It cures readily at ambient temperatures or more rapidly at elevated temperatures. To optimize the properties, the best cure schedule is overnight at room temperature, followed by 2-3 hours at 150-200°F.

EP42HT-4AOMed Black has good thermal conductivity, while still maintaining excellent electrical insulation values. It bonds well to a wide variety of substrates, including metals, composites, glass, ceramics, rubbers and plastics. Since this system contains filler, an added benefit is enhanced dimensional stability and very low shrinkage upon curing. EP42HT-4AOMed Black has lower exotherm and is castable to thicknesses up to and exceeding 2-3 inches. EP42HT-4AOMed Black has stellar resistance to repeated autoclaving, radiation and aggressive chemical sterilants. This epoxy is also notable in that it is cryogenically serviceable. Its temperature range is 4K to +400°F. It is most likely to be considered in specialty medical device applications.

Product Advantages

  • Relatively easy handling
  • Long working life
  • Conducts heat while still electrically insulative
  • Cryogenically serviceable
  • Can resist higher temperatures
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.