Two part, thermally conductive epoxy for medical device manufacturing

Key Features

  • Exceptional heat resistance
  • Thermally conductive and electrically insulative
  • Cryogenically serviceable
  • Passes ISO 10993-5 and USP Class VI

Product Description

Master Bond EP42HT-4AOMed Black is a two component epoxy adhesive, sealant, coating and casting system with a number of noteworthy features. It has a forgiving mix ratio of 100 to 40 by weight along with very good flow properties. It cures readily at ambient temperatures or more rapidly at elevated temperatures. To optimize the properties, the best cure schedule is overnight at room temperature, followed by 2-3 hours at 150-200°F.

EP42HT-4AOMed Black has good thermal conductivity, while still maintaining excellent electrical insulation values. It bonds well to a wide variety of substrates, including metals, composites, glass, ceramics, rubbers and plastics. Since this system contains filler, an added benefit is enhanced dimensional stability and very low shrinkage upon curing. EP42HT-4AOMed Black has lower exotherm and is castable to thicknesses up to and exceeding 2-3 inches. EP42HT-4AOMed Black has stellar resistance to repeated autoclaving, radiation and aggressive chemical sterilants. This epoxy is also notable in that it is cryogenically serviceable. Its temperature range is 4K to +400°F. It is most likely to be considered in specialty medical device applications.

Product Advantages

  • Relatively easy handling
  • Long working life
  • Conducts heat while still electrically insulative
  • Cryogenically serviceable
  • Can resist higher temperatures

Industrial Certifications


USP Class VI Medical

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

Packaging


Cans

Pails

EP42HT-4AOMed Black is available is various sizes and units to accommodate customer's needs.