MasterSil 151S

Two part, silver filled, low outgassing silicone for bonding, sealing and coating
Key Features
  • Excellent electrical conductivity
  • Addition cured type system
  • Highly flexible & temperature resistant
  • NASA low outgassing
Typical Properties
Viscosity
Part A: paste, Part B: 50-150 cps
Cure Schedule
4-6 hours at 150 to 180°F and 2-3 hours at 190 to 210°F
Hardness
80-90 Shore A
Service Temperature Range
-80°F to +400°F
Elongation
100-150%
Volume Resistivity
0.004 ohm-cm
תמונה
MasterSil 151S Two Part Silicone System
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond MasterSil 151S is a two component, silver filled silicone with superb electrical conductivity along with good heat transfer properties. Part A has a smooth, paste consistency, Part B is a low viscosity liquid. The mix ratio is 100 to 5 by weight. Upon mixing, MasterSil 151S retains its smooth, paste consistency. The working life for a 50 gram mass is 6 to 12 hours. The best cure schedule options are 4-6 hours at 150 to 180°F and 2-3 hours at 190 to 210°F. The system has low shrinkage upon curing and reasonably good dimensional stability.

MasterSil 151S bonds well to a wide variety of substrates including metals, ceramics, glass, composites as well as many types of rubber and plastics. The system has very good flexibility and elongation. Consequently, it can withstand aggressive thermal cycling as well as mechanical and thermal shocks. Its paste consistency allows it to be easily applied as an adhesive, sealant or coating. It can also be utilized as a form-in-place conductive gasketing material. Since it is an addition cured system it cures readily in thicknesses up to and beyond 1/4 inch thick. The color of Part A is silver and Part B is clear. The service temperature range is -80°F to +400°F. MasterSil 151S is most likely to be considered in aerospace, electronic, opto-electronic and specialty OEM applications, where excellent electrical conductivity, resounding flexibility, high temperature resistance and low outgassing, are necessary requirements.

Product Advantages

  • After mixing, paste consistency
  • Exceptionally long working life
  • Cures well in deep and wide sections
  • Very good electrical conductivity
  • Vacuum compatible
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.