EP17HTDA-2

One component die attach epoxy system with exceptionally high glass transition temperature
Key Features
  • Not premixed and frozen
  • Paste consistency
  • Thermally conductive, electrically insulating
  • High compressive strength
Typical Properties
Viscosity
>1,000,000 cps
Cure Schedule
4-5 hours at 300°F or 3-4 hours at 350°F; to optimize properties, use an additional 2-3 hours at 400°F
Hardness
90-95 Shore D
Service Temperature Range
-80°F to +600°F
Dielectric Constant
4.4
Glass Transition Temperature (Tg)
185-190°C
תמונה
One Part Die Attach Epoxy EP17HTDA-2
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP17HTDA-2 is a one component, heat cured epoxy system for bonding, sealing, and die attach applications. It does not require any mixing and the curing temperature is 300-350°F. It is not premixed and frozen and has an unlimited working life at room temperature. It will cure in either 4-5 hours at 300°F or 3-4 hours at 350°F. To optimize properties, use one of the above cure schedules plus an additional 2-3 hours at 400°F. Its viscosity and flow allow it be an effective adhesive for die attach applications.

EP17HTDA-2 bonds well to a wide variety of substrates such as metal, ceramics, plastics and composites. It has an impressive array of physical strength properties, particularly tensile modulus, compressive strength and glass transition temperature. The system is thermally conductive and electrically insulative. It is highly chemically resistant to water, acids, bases, solvents, fuels, and oils. It has superb electrical insulation along with good thermal conductivity. The service temperature range is from -80°F to +600°F. The standard color is off white. EP17HTDA-2 is recommended for specialty type applications where its exceptionally high Tg of 185-190°C is a critical factor in die attach applications.

Product Advantages

  • Single component system
  • Thermally conductive, electrically insulative
  • Can withstand temperatures used in electronic packaging such as wire bonding
  • DIspenses well for die attach applications
  • NASA low outgassing
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.