UV26SP
One part, low viscosity UV curable system featuring high temperature resistance for bonding, sealing and coating
Key Features
- Excellent physical strength properties
- High glass transition temperature
- Superb chemical resistance
- No oxygen inhibition
- Meets NASA low outgassing specifications
Typical Properties
Viscosity
250-1,500 cps
Cure Schedule
UV light 320-365 nm for 10-20 seconds
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +500°F
Glass Transition Temperature (Tg)
160 to 170°C
Refractive Index
1.55