EP110F8-1
Two component, high performance epoxy for potting, sealing, encapsulating and casting
Key Features
- Exceptionally long working life at room temperature
- Low viscosity
- Outstanding electrical insulation properties
- Highly resistant to thermal cycling and shock
Typical Properties
Viscosity
2,500-5,000 cps
Cure Schedule
4-6 hours at 250-300°F
Hardness
65-75 Shore D
Service Temperature Range
-80°F to +325°F
Dielectric Constant
2.81
Elongation
85-95%