EP17HT-3

One component, snap-curing epoxy system
Key Features
  • Snap curing
  • High temperature resistance up to +400°F
  • Can cure in sections up to ¼ inch thick
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
80,000-130,000 cps
Cure Schedule
300°F for 8-12 minutes, 350°F for 3-5 minutes
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +400°F
Glass Transition Temperature (Tg)
110-120°C
Tensile Lap Shear Strength
1,800-2,000 psi
תמונה
EP17HT-3 One Part Snap Curing Epoxy
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Product Description

Master Bond EP17HT-3 is a one part epoxy that fully cures in 3-5 minutes at 350°F. It is capable of service up to +400°F with excellent strength retention properties. Also, unlike many other one part epoxies, EP17HT-3 can be cured in sections up to ¼ inch thick. EP17HT-3 is 100% reactive and contains no solvents or diluents. As a one part system, it not only requires no mixing, but the working life is "indefinite”. It will not gel until heated above 200°F. EP17HT-3 has excellent electrical insulation characteristics, superior chemical resistance and outstanding physical properties. It is yellow to brown in color. There is a paste version called EP17HT-3ND2 as well as a slightly toughened formulation called Supreme 17HT-3 which offers enhanced resistance to thermal cycling and thermal and mechanical shock.

Product Advantages

  • One part system; no mixing required; contains no solvents or diluents
  • Snap cure: Sets up in 20-30 seconds and fully cures in 3-5 minutes at 350°F
  • Superior temperature resistance; serviceable up to +400°F
  • Outstanding electrical insulation properties and chemical resistance
  • Can cure in sections up to ¼ inch thick
  • Easy application: Unlimited working life—will not set up at room temperature
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.