EP17HTDA-1

One component, high temperature resistant epoxy system for bonding and sealing
Key Features
  • Ideal for die attach applications
  • Will tack in 5 to 15 minutes
  • Meets MIL-STD-883J Section 3.5.2 for thermal stability
  • Meets NASA low outgassing specifications
Typical Properties
Viscosity
200,000-250,000 cps
Cure Schedule
12-15 minutes at 212°F or 5-6 minutes at 300°F, followed by 2-3 hours at 300°F or 1-2 hours at 350°F
Hardness
85-95 Shore D
Service Temperature Range
-80°F to +525°F
Dielectric Constant
4.3
Glass Transition Temperature (Tg)
130-135°C
תמונה
EP17HTDA-1 One Part Epoxy
Certifications

MIL-STD-883J for Thermal Stability

ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP17HTDA-1 is a one component, heat cured epoxy system primarily for die attach applications as well as more conventional bonding and sealing. It requires no mixing and cures readily at 300-350°F. It is not premixed and frozen and has an unlimited working life at room temperature. This epoxy will tack reasonably fast, 12-15 minutes at 212°F, 5-6 minutes at 300°F. This is followed by curing at either 2-3 hours at 300°F or 1-2 hours at 350°F, in order to optimize properties. EP17HTDA-1 has excellent consistency and flow for die attach applications.

This epoxy system features excellent physical properties, superb electrical insulation along with good thermal conductivity, even at elevated temperatures. This system is also distinctive in that it has a relatively low exotherm upon curing. EP17HTDA-1 is 100% reactive and contains no solvents or diluents. EP17HTDA-1 bonds well to similar and dissimilar substrates such as metal, ceramics, plastics and composites. It has a noteworthy resistance to many chemicals including acids, bases, salts, fuels, oils and many solvents. Significantly, it has minimal shrinkage upon curing. Its service temperature range is from -80°F to +525°F. Since it passes NASA low outgassing, it can be used in vacuum type situations and other applications where that requirement is needed. EP17HTDA-1 is used primarily as a die attach and adhesive/sealant in electronic and related applications, where high temperature resistance, good electrical insulation properties and thermal conductivity are desirable.

Product Advantages

  • Single component system
  • Thermally conductive, electrically insulative
  • Excellent die shear strength
  • High temperature resistance
  • Ideal viscosity flow profile for die attaching
  • Fast tacking
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.