EP30Med

Low viscosity, two component epoxy system
Key Features
  • Biocompatible as per USP Class VI testing
  • Passes ISO 10993-5 for cytotoxicity
  • Meets certification for indirect contact with food
  • Resistant to chemical sterilants
  • Optically clear
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 900-1,500 cps, Part B: 280-500 cps
Cure Schedule
overnight at 75°F, followed by 1-2 hours at 150-200°F
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Strength
440 volts/mil
Tensile Modulus
300,000-350,000 psi
תמונה
EP30Med Two Part Epoxy
Certifications

FDA Food Grade 21 CFR 175.105

ISO 10993-5 for Cytotoxicity

Meets EU Directive 2015/863

USP Class VI Medical

1,000 Hours at 85°C/85% RH

Product Description

Master Bond EP30Med is a two component, optically clear, low viscosity epoxy resin system for high performance bonding, sealing, coating, and encapsulating. It is formulated to cure readily at room temperature or more quickly at elevated temperatures. It has a four to one mix ratio by weight and contains no solvents or diluents. EP30Med produces high strength, rigid bonds which are very resistant to chemicals including water, oils and many organic solvents, as well as cold sterilants, EtO and gamma radiation. It is serviceable over the wide temperature range of -60°F to +250°F. It bonds well to a wide variety of substrates including metals, glass, ceramics, wood and many plastics. EP30Med has exceptionally low linear shrinkage upon cure. The cured compound is also an outstanding electrical insulator. The combination of these properties makes this system well suited for encapsulating and potting applications. Most importantly, EP30Med meets USP Class VI specifications, making it ideal for a variety of uses in medical devices. EP30Med also meets FDA requirements for indirect food contact as per FDA CFR 175.105. To optimize the properties and to attain desired biocompatibility, the recommended cure schedule is overnight at room temperature, followed by 1-2 hours at 150-200°F.

Product Advantages

  • Easy mixing: four to one by weight
  • Convenient application: low viscosity; only contact pressure required for cure
  • Versatile cure schedules: room temperature curing, or faster at elevated temperatures
  • Forms high strength, rigid bonds to a wide variety of substrates
  • Exceptionally low shrinkage
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.