EP3HTS

One part, electrically conductive epoxy system
Key Features
  • Low volume resistivity
  • High tensile shear strength
  • Thermally conductive
  • Silver conductive epoxy adhesive
  • Rapid cures at moderate temperatures
  • Superior bond strength
Typical Properties
Viscosity
paste
Cure Schedule
45-90 minutes at 250°F or 20-40 minutes at 300°F
Hardness
65 Shore D
Service Temperature Range
-60°F to +400°F
Tensile Lap Shear Strength
>400 psi
Volume Resistivity
<0.001 ohm-cm
תמונה
EP3HTS One Part Epoxy
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP3HTS is a one component, silver filled, electrically conductive epoxy system combining excellent physical strength and temperature resistance values along with a fast cure schedule. EP3HTS has truly exceptional conductivity; less than 1 milliohm-cm. As mentioned above, EP3HTS is a single component system with no mixing needed and curing is accomplished by heating. Typical curing schedules are 45-90 minutes at 250°F or 20-40 minutes at 300°F. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics and many plastics. EP3HTS has fine dimensional stability. It has very good chemical resistance to water, oils, fuels and cleaning agents. Some of the positive features of this system from a handling perspective are its smooth paste consistency and that it is dispensable from a syringe. The service temperature range is -60°F to +400°F. The merging of terrific electrical conductivity, no mixing, fast curing and superior physical properties enable EP3HTS to be an excellent selection for aerospace, electronic, microelectronic, optical and related applications, particularly where curing time considerations are paramount.

Product Advantages

  • Single component system; no mixing prior to use, smooth paste consistency
  • Easy to apply, dispenses easily and consistently from syringes
  • Fast curing, well suited for rigorous manufacturing applications
  • Bonds well to a wide variety of substrates
  • Excellent electrical and thermal conductivity
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.