EP3HTSCN

One part, high performance, electrically conductive epoxy
Key Features
  • Very good electrical conductivity
  • Cures rapidly cures at moderately elevated temperatures
  • Excellent bonding properties
  • Good thermal conductivity
Typical Properties
Viscosity
paste
Cure Schedule
cures readily at 250°F at 45-50 minutes or in just 20-30 minutes at 300°F
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +400°F
Tensile Lap Shear Strength
900-1,100 psi
Volume Resistivity
0.05 to 0.10 ohm-cm
תמונה
EP3HTSCN One Part Epoxy
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond EP3HTSCN is a one component, silver coated nickel filled, electrically conductive epoxy system combining excellent physical strength properties as well as convenient handing. EP3HTSCN is not premixed and frozen and has an unlimited working life at room temperature. As mentioned above, EP3HTSCN is a single component system with no mixing needed and curing is accomplished by heating. EP3HTSCN cures readily at 250°F at 45-50 minutes or in just 20-30 minutes at 300°F. This system features a volume resistivity of 0.05 to 0.10 ohm-cm.

It adheres well to a wide variety of substrates including metals, composites, ceramics, glass and many plastics. EP3HTSCN has fine dimensional stability. It has reasonably good chemical resistance to water, oils, fuels and cleaning agents. It has a smooth paste consistency and is readily dispensable from a syringe. Its service temperature range is from -60°F to +400°F. EP3HTSCN combines electrical conductivity, relatively simple processing along with a very good physical strength profile. EP3HTSCN is an excellent choice for aerospace, electronic, microelectronic, optical, specialty OEM and related applications, where simple handling, fast curing and reliability are needed.

Product Advantages

  • Single component system; no mixing prior to use, smooth paste consistency
  • Dispenses easily and consistently from syringes
  • Fast curing, well suited for rigorous manufacturing applications
  • Bonds well to a wide variety of substrates
  • Excellent electrical and thermal conductivity
  • Lower volume resistivity
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.