EP3RR-1
One component epoxy for potting, encapsulation and underfill applications
Key Features
- Good flow properties
- Thermally conductive and electrically insulating
- Can be cast in thicknesses up to 1 inch
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
10,000-40,000 cps
Cure Schedule
250°F for 20-30 minutes; 300°F for 10-15 minutes
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +350°F
Dielectric Constant
4.5
Dielectric Strength
450 volts/mil
Thermal Conductivity
7-8 BTU•in/(ft²•hr•°F) [1.01-1.15 W/(m•K)]
Volume Resistivity
>10¹⁴ ohm-cm