EP46CA-1

Two component epoxy for structural bonding featuring superlative heat resistance; requires oven curing
Key Features
  • Long pot life at room temperature
  • High bonding strength
  • Service temperature range of -100°F to +500°F
  • Outstanding electrical insulation properties
Typical Properties
Viscosity
5,000-20,000 cps
Cure Schedule
250-300°F for 2-3 hours, post cure for optimum properties at 350-400°F for 2 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +500°F
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
160-170°C
Volume Resistivity
>10¹⁶ ohm-cm
תמונה
EP46CA-1 Two Part Epoxy
Applications
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP46CA-1 is a two part epoxy system for high performance structural bonding and sealing, suitable for applications where resistance to temperatures from -100°F to +500°F is required. It is 100% reactive and does not contain any solvents or diluents. While it does not cure at room temperature, it does cure readily at elevated temperatures. A good curing schedule to optimize properties is 2 hours at 300°F, followed by a few hours at 350-400°F. The cured epoxy produces bonds and seals with high mechanical strength and excellent chemical resistance. EP46CA-1 has a forgiving 100 to 50 mix ratio by weight. It should be noted that EP46CA-1 is relatively exothermic and should not be cured in sections greater than 10-20 thousandths of an inch thick and a bond line thickness is typically 2-6 thousandths of an inch.

Although EP46CA-1 is primarily used for structural bonding, it is also a superb choice as a matrix resin for fiber reinforced, high performance, heat resistant composite structures. It can withstand intense thermal cycling and resist many chemicals, including water, oils, solvents, bases and acids. It bonds exceptionally well to metals, composites, glass, ceramics and many plastics. Once cured, the system is a top flight electrical insulator. The color of Part A is black and Part B is moderately dark brown. EP46CA-1 is normally used in demanding applications found in the aerospace, electronic and specialty OEM industries where exceptional thermal and chemical resistance might be required.

Product Advantages

  • Easy application: contact pressure only required for cure, system spreads evenly and smoothly
  • Convenient cure schedules at elevated temperatures
  • Outstanding heat resistance and thermal stability
  • Robust chemical resistance
  • First rate electrical insulation properties even upon prolonged exposure to hostile environments
  • Working life over 24 hours at room temperature
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.