EP46HT-2

Two part high performance epoxy for bonding, sealing, coating and casting
Key Features
  • Long working life
  • Service temperature range from -100°F to +500°F
  • Resists prolonged exposure to hostile environments
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
12,000-20,000 cps
Cure Schedule
250-300°F, 3-4 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +500°F
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
155-165°C
תמונה
EP46HT-2 Two Part Epoxy
Certifications

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Product Description

Master Bond EP46HT-2 is a versatile two component epoxy system that can be used for bonding, sealing, coating and casting. It is most prominent for its temperature resistance along with the capability of withstanding aggressive chemicals. Its service temperature range extends from -100°F to +550°F. It is 100% reactive and does not contain any solvents or diluents. It is formulated to cure rapidly and requires a minimum curing temperature of 250°F; although a variety of cure schedules are possible. It should be noted that the mix ratio is a very forgiving 100 to 30-35 parts by weight. Upon curing, EP46HT-2 has a wide array of impressive physical and mechanical properties. It bonds well to a variety of substrates including metals, composites, ceramics, glass, rubbers and many plastics. One of the more noteworthy attributes of this system is its chemical resistance profile, which includes the ability to withstand many acids, bases, oils, fuels, hydrocarbons and solvents. It is also a very good electrical insulator. Unlike the EP46HT-1 product series, this line is not exothermic and can be used for potting and encapsulation. The color of Part A is clear; the color of Part B is brown. Master Bond EP46HT-2 is primarily used in specialty aerospace, electronic, petrochemical and OEM applications where high temperature resistance and the ability to withstand hostile chemicals is desirable.

Product Advantages

  • Very forgiving mix ratio
  • Long open time at room temperature
  • Excellent thermal stability
  • Capable of withstanding aggressive chemicals
  • Good physical strength properties
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.