EP46HT-2AO Black

Two part high performance epoxy for bonding, sealing and encapsulation
Key Features
  • Long working life
  • Thermally conductive, electrically insulative
  • Passes NASA low outgassing test requirements
  • High temperature resistance
Typical Properties
Viscosity
140,000-280,000 cps
Cure Schedule
3-4 hours at 250-300°F followed by a post cure of 2-3 hours at 350-400°F
Hardness
85-90 Shore D
Service Temperature Range
-100°F to +500°F
Dielectric Strength
450 volts/mil
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
EP46HT-2AO Black Two Part Epoxy
Certifications

MIL-STD-810G for Fungus Resistance

ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP46HT-2AO Black is a two component epoxy system for demanding bonding, sealing and encapsulation applications where thermal conductivity, electrical insulation and high temperature resistance are required. It is 100% reactive and does not contain any solvents or diluents. EP46HT-2AO Black is formulated to cure rapidly and requires a cure temperature of 250°F or more. An optimal curing schedule is 3-4 hours at 250-300°F followed by a post cure of 2-3 hours at 350-400°F. The glass transition temperature is quite high, between 140-150°C, and the service temperature range is -100°F to +500°F. Once cured, EP46HT-2AO Black features exceptional physical and mechanical properties, along with exquisite dimensional stability. It bonds well to a wide variety of substrates including metals, glass, ceramics, composites, various rubbers and many plastics. It is a highly functional electrical insulator. It has very good chemical resistance to water, fuels, oils, acids and bases. Most importantly, it passes NASA low outgassing testing. The color of Part A is black and Part B is gray. This high powered combination of product properties allows this system to be used in challenging applications in aerospace, electronics, optoelectronics and in vacuum environments.

Product Advantages

  • Extremely forgiving mix ratio
  • Very long open time at room temperature
  • Top notch heat resistance
  • Thermally conductive, electrically insulative
  • High quality dimensional stability
  • Meets NASA low outgassing requirements
  • Passes fungus resistance MIL-STD-810G
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.