EP51ND

Fast setting, two component epoxy for bonding and sealing
Key Features
  • Easy handling
  • Paste consistency
  • Bonds well to a wide variety of substrates
  • Cryogenically serviceable
Typical Properties
Viscosity
Part A: paste, Part B: 50,000-100,000 cps.
Cure Schedule
Full cure occurs in about 24 hours at 75°F
Hardness
70-80 Shore D.
Service Temperature Range
4K to +250°F .
Dielectric Constant
4.7.
Dielectric Strength
425 volts/mil.
תמונה
EP51ND Two Part Epoxy
Applications
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond EP51ND is a high performance epoxy featuring faster curing, convenient handling, and sound properties after cure. This nondrip system has a forgiving one to one mix ratio by weight or volume. EP51ND will generally set up sufficiently in about 10-15 minutes so that the bonded parts can be removed from a fixture or clamp. Full cure occurs in about 24 hours. EP51ND does not contain any solvents or diluents. Upon curing, it has very low shrinkage and good dimensional stability.

glass, ceramics, vulcanized rubbers, and many plastics. It can withstand rigorous thermal cycling as well as thermal shock. EP51ND is electrically and thermally isolating. Its temperature range is from 4K to +250°F and it has been used in a number of demanding cryogenic applications. An interesting feature is that it can be mixed and cured at temperatures as low as 50-60°F. Although curing is muchslower than at ambient temperatures, the system will fully cure in 3-5 days. The Color of Part A is amber and Part B is amber clear. There is another version where the A and B are color coded, called EP51ND-3. Here, Part A is black, Part B is white, and upon mixing, the final product is gray. Color coding is especially useful in determining if the epoxy is completely mixed.EP51ND is a versatile system that can be used in standard OEM, aerospace, optical, electronic, cryogenic, and field applications where a reliable and robust system is required.

Product Advantages

  • Non-critical one to one mix ratio by weight or volume
  • Easy to apply, paste like consistency
  • High bond strength to a wide variety of substrates
  • Available in various viscosities and colors
  • Serviceable at cryogenic temperatures down to 4K
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.