EP5G-80

One component, graphite filled epoxy with a curing temperature of 80°C
Key Features
  • Good electrical and thermal conductivity
  • Thixotropic paste
  • Not premixed and frozen
  • NASA low outgassing
Typical Properties
Viscosity
30,000-300,000 cps
Cure Schedule
4 hours at 80°C
Hardness
75-85 Shore D
Service Temperature Range
-58°F to +347°F
Glass Transition Temperature (Tg)
130-140°C
Volume Resistivity
5-15 ohm-cm
תמונה
EP5G-80 One Component Epoxy
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Product Description

Master Bond EP5G-80 is a one component, graphite filled epoxy paste for bonding, sealing and coating applications. It is electrically and thermally conductive. The system has outstanding physical strength properties, stellar dimensional stability and low shrinkage upon curing. It is not premixed and frozen, and has a working life of 8-12 hours at room temperature. Curing is simple and straightforward, 4 hours at 80°C.

EP5G-80 bonds well to a wide variety of substrates such as metals, composites, ceramics and many plastics. It has a remarkably high tensile modulus and compressive strength. The electrical conductivity is quite robust, with a volume resistivity between 5 to 15 ohm-cm. This exceptionally low volume resistivity allows EP5G-80 to be utilized in applications outside of the typical ones for graphite filled epoxies (e.g. static dissipation, EMI/RFI shielding). Such a low resistance permits the system to be used for direct connection of substrates where this property is required. Graphite is a desirable filler material because of its performance and cost effectiveness. EP5G-80 will resist water, oils and fuels. Its color is black. The service temperature range is -50°C to +175°C. A particularly advantageous feature of EP5G-80 is, it is highly screen printable. It can be used in electronic, aerospace, medical device, optical and specialty OEM type applications where a non-metallic, conductive epoxy is needed. Some recent applications for graphite filled epoxy involve lithium ion batteries, fuel cells as well as carbon brushes.

Product Advantages

  • Convenient handling
  • Non-metallic filler
  • Thermal and electrical conductivity
  • Good lubricity
  • Low coefficient of thermal expansion
  • Passes NASA low outgassing specifications
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.