EP62-1AO

Two component epoxy resin system featuring excellent temperature and chemical resistance
Key Features
  • Long open time at room temperature
  • Cures rapidly at moderate temperatures
  • Thermally conductive, electrically insulating
  • NASA low outgassing
Typical Properties
Viscosity
paste
Cure Schedule
4-6 hours at 140-160°F, 20-40 minutes at 175-200°F or 10-20 minutes at 250-300°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.8
Tensile Lap Shear Strength
800-1,000 psi
תמונה
Two Component Epoxy EP62-1AO
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Product Description

Master Bond EP62-1AO is a two component, flowable epoxy system with an exceptionally long open time at ambient temperature. It has a forgiving 100 to 10 mix ratio by weight. The pot life of 100 grams is 12-14 hours. Typical cure schedule options are 4-6 hours at 140-160°F, 20-40 minutes at 175-200°F or 10-20 minutes at 250-300°F. To obtain optimum properties, post curing at 200-300°F for 2-4 hours is recommended. EP62-1AO gels at room temperature in about 24 hours and it will not reliquify when the elevated temperature is added to complete the cure.

EP62-1AO bonds well to a wide variety of substrates including metals, glass, ceramics, composites and many plastics and rubbers. When compared to other thermally conductive epoxies, it is noteworthy that EP62-1AO has a better chemical resistance profile to acids, bases, and solvents. The service temperature range is -60°F to +450°F. The color of Part A is off white and Part B is dark brown. EP62-1AO is used for aerospace, electronic, optical, specialty OEM and related applications, particularly when high temperature resistance, thermal conductivity along with electrical insulation are required.

Product Advantages

  • Forgiving 100 to 10 mix ratio by weight
  • Long working life
  • Versatile curing schedules
  • Very good chemical resistance
  • Wide service temperature range
  • Low coefficient of thermal expansion
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.