MasterSil 151
Two component, addition curing silicone for potting, encapsulation and sealing
Key Features
- Optically clear
- Electrically insulative
- Low viscosity
- Serviceable from -65°F to +400°F
- Cures at room or elevated temperatures
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 2,000-4,000 cps, Part B: 50-150 cps
Cure Schedule
75°F 24-48 hours; 200°F 1-2 hours
Hardness
50-60 Shore A
Service Temperature Range
-65°F to +400°F
Dielectric Strength
450 volts/mil
Refractive Index
1.436