MasterSil 156
Two part silicone for high performance potting, encapsulation and sealing
Key Features
- Superior thermal conductivity
- Superb electrical insulation properties
- Flame retardant UL 94V-0
- Low exotherm; very long pot life
- Can cure in thicknesses up to and beyond 1-2 inches
- UL temperature rated up to 105°C
Typical Properties
Viscosity
35,000-50,000 cps
Cure Schedule
1-2 hours at 250°F
Hardness
50-60 Shore A
Service Temperature Range
-65°F to +221°F
Dielectric Strength
450 volts/mil
Elongation
120-150%
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
Meets EU Directive 2015/863
UL 94V-0 Flame Resistant
Packaging
וידאו
Thermally Conductive, Flame Retardant Silicone System Video
High temperature resistance and flexibility are all wrapped up into one in this two part silicone.
MasterSil 156 is ideal for potting and encapsulation with its lower viscosity and excellent flow. See its other attributes in this animated video.