Thermally Conductive, Flame Retardant Silicone System Video

High temperature resistance and flexibility are all wrapped up into one in this two part silicone. MasterSil 156 is ideal for potting and encapsulation with its lower viscosity and excellent flow. See its other attributes in this animated video.

Video Transcript

Silicone polymer systems typically combine high temperature resistance with outstanding flexibility. MasterSil 156 does all that and more.

This two part silicone features a lower viscosity and excellent flow, making it ideal for potting and encapsulation. It meets UL94V-0 for flame retardancy, and has both superior thermal conductivity, and electrical insulation. With a convenient one to one mix ratio by weight, it can cure in thickness up to and beyond 1-2 inches. It also has very low shrinkage upon cure. MasterSil156 bonds well to a wide variety of substrates including metals, composites, glass, ceramics and many rubbers and plastics. Due to its flexibility, it resists vibration and shock. It also resists water, humidity and oils.

Thanks for joining us. For information, please contact a technical advisor.

Featured Product Covered in this Video