MasterSil 713

Low viscosity, one component silicone elastomer compound
Key Features
  • Fast, room temperature cures
  • Ideal for smaller encapsulations
  • Well suited for conformal coatings
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
2,000-4,000 cps
Cure Schedule
Tack-free time, 75°F, >50% humidity 12-16 minutes
Hardness
20-30 Shore A
Service Temperature Range
-75°F to +400°F
Dielectric Constant
2.5
Elongation
200-300%
תמונה
MasterSil 713 One Part Silicone
Certifications

1,000 Hours at 85°C/85% RH

Meets EU Directive 2015/863

Packaging
Product Description

MasterSil 713 is an easy to use, one component high performance silicone system with exceptionally low viscosity for bonding, sealing, coating, encapsulations and formed-in-place gaskets. This self leveling system bonds well to a wide variety of substrates including glass, metals and many plastics. MasterSil 713 is a faster curing system, in which the speed of cure depends upon the level of humidity and the thickness of the layer being cured. The thicker the layer, the slower the rate of cure. MasterSil 713 can be cured in thicknesses up to ¼ inch deep with superb flexibility and elasticity. Additionally, it is an outstanding electrical insulator. It has a service temperature range of -75°F to +400°F. Its low viscosity also enables this system to be used as a conformal coating. MasterSil 713 is completely non-corrosive and safe to use with electronics, optoelectronics, etc.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.