MasterSil 920-LO

One part, low outgassing, low stress silicone system for coating, sealing & encapsulating
Key Features
  • Meets NASA ASTM E595
  • Moderate viscosity with good flow properties
  • Neutral type cure
  • Superb optical clarity
Typical Properties
Viscosity
5,000-10,000 cps
Cure Schedule
Recommended cure time, 75°F: 7 days
Hardness
25-35 Shore A
Service Temperature Range
-175°F to +500°F
Dielectric Constant
2.5
Refractive Index
1.43
תמונה
MasterSil 920-LO One Part Silicone System
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Packaging
Product Description

MasterSil 920-LO is a high performance, RTV silicone for sealing, coating and small encapsulations. First and foremost, it meets NASA low outgassing specifications. It is a neutral curing, non-corrosive type system. Also it has very good flow properties and outstanding electrical insulation values. These properties facilitate its use as a conformal coating and encapsulation system. With a softer durometer than many other silicones, it is particularly well suited for protecting sensitive electronic components. In fact, since it is low outgassing and optically clear, it can be used for select optical applications where delicate components must be protected. Similar to other one part silicones, the curing mechanism is based on humidity; the higher it is, the faster the cure. Also thinner sections cure more quickly than thicker ones. Another noteworthy property is its wide service temperature range of -175°F to +500°F. MasterSil 920-LO bonds very well to a wide variety of substrates including metals, glass as well as many plastics and rubber materials. With its inherent robust flexibility, the system can withstand the most rigorous kinds of thermal cycling and shock. MasterSil 920-LO is a “go-to material” in the encapsulation of sensitive electronic and optical components, especially when low outgassing and low stress are critical requirements. It should be noted, in order to achieve the low outgassing properties, a seven day cure at room temperature is recommended.

Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.