MB600

One component sodium silicate, aqueous based bonding and coating system
Key Features
  • High temperature resistance up to 1,500°F
  • Strong rigid bonds
  • Water based system, relatively non-toxic
  • Highly transparent
Typical Properties
Viscosity
30-600 cps
Cure Schedule
45 minutes at 200°F followed by another 60 minutes at 300-400°F
Service Temperature Range
0°F to 1,500°F
Specific Gravity
1.53
Volume Resistivity
>10¹⁰ ohm-cm
תמונה
MB600 Sodium Silicate System
Applications
Certifications

Meets EU Directive 2015/863

Packaging
Product Description

Master Bond MB600 is an aqueous based sodium silicate system for bonding and coating. Most noteworthy is its high temperature resistance—serviceable up to 1,500°F. This one component, low viscosity system bonds well to a wide variety of substrates including, metal, glass, ceramics, composites and many plastics. This system, which is often generically referred to as water glass, can eventually cure at ambient temperatures but heat curing is greatly preferred to optimize properties. A widely used cure schedule is 45 minutes at 200°F followed by another 60 minutes at 300-400°F. Special care should be taken to avoid rapid heating as this may cause the system to “blister”. It is advisable to ramp up temperatures over a 15-30 minute span. It is colorless, odorless, non-flammable and relatively non-toxic. After curing, it retains its optical clarity and has very special light transmission properties, particularly in the range of 200-350 nm.

One aspect of MB600 is that the degree of curing can be utilized in an unusual manner. If it is 70-90% “fully cured” it still contains water, but will have attained most of its strength and temperature resistance properties. The adhesive can then actually be removed at this juncture if it is exposed to boiling water for a number of hours. If and when it is more fully cured, it will totally resist the boiling water. This confers a removability factor to the system when processed in the manner described above. It also should be noted that MB600 is highly alkaline and can adversely affect or etch certain types of substrates, especially glass. MB600 has sound electrical insulation properties and good dimensional stability. While silicates in general have a huge range of applications, MB600 is a more specialized system in the silicate family and is formulated for use in optical, opto-electronic, aerospace, electronic and specialty types of OEM applications.

Product Advantages

  • Great temperature resistance
  • Winning optical transmission properties, even at 200-350 nm
  • Bonds well to a wide variety of substrates
  • Highly effective moisture barrier
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.