Super Gel 9

Two component urethane modified epoxy gel-like system
Key Features
  • Cures to a low Shore A hardness
  • Convenient handling
  • Room temperature curing
  • Relatively easy to remove
Typical Properties
Viscosity
3,000-9,000 cps
Cure Schedule
cures at 75°F, 4-7 days
Hardness
<5 Shore A
Service Temperature Range
-100°F to +200°F
Dielectric Strength
>420 volts/mil
Refractive Index
1.5253
תמונה
Super Gel 9 Two Part Urethane Modified Epoxy
Product Description

Master Bond Super Gel 9 is a two component, urethane modified epoxy system that cures readily at room temperature to form a soft, resilient, gel-like system with good dimensional stability. Its hardness is exceptionally low, about 5-10 Shore A. One can accomplish retrievability with a sharp knife or razor blade and Super Gel 9 will not shatter. It has a very convenient two to one mix ratio by weight or volume, along with an extremely low viscosity and exotherm enabling it to be cast in larger sections up to 2-3 inches thick. Super Gel 9 is amber and optically clear. The combination of its easy handling and cured properties enables this versatile system to be used in a variety of applications, especially the encapsulation of sensitive electronic parts and sealing delicate optical components. It can also be used in acoustical applications where dampening properties may be desirable. This exceptional softness allows it to be easily repairable and confers it with unsurpassed thermal cycling and mechanical shock resistance.

Super Gel 9 bonds well to an array of substrates, such as metals, glass, ceramics and many rubbers and plastics. It has a remarkably long working life of 7-9 hours depending on the mass that is mixed (the smaller the mass, the longer the working life). It has good resistance to water and oils. The service temperature range is -100°F to +200°F. The color of both Parts A and B are clear. This multi-functional system is widely used in the aerospace, electronic, optical, electro-optical and other specialty industries where this unique blend of properties is needed.

Product Advantages

  • Easy handling; two to one mix ratio by weight or volume; low viscosity
  • Very low exotherm; remarkably long working life
  • Exceptionally soft and resilient
  • Good dimensional stability
  • Easily repairable; widely used for retrieving components
  • Often used in conjunction with sensitive electronic and optical components
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.