Supreme 112
Two part epoxy for bonding, sealing, potting and impregnation requires elevated temperature curing
Key Features
- Very low viscosity
- High temperature resistance
- Exceptionally long open time
- Passes NASA low outgassing
Typical Properties
Viscosity
50-200 cps
Cure Schedule
1-2 hours at 200-210°F followed by 3-4 hours at 250°F and then 4-6 hours at 300°F
Hardness
75-90 Shore D
Service Temperature Range
-80°F to +550°F
Glass Transition Temperature (Tg)
190-195°C
Volume Resistivity
>10¹⁴ ohm-cm at 25°C, >10¹² ohm-cm at 150°C
תמונה
Discuss with a Specialist
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
(1-2 Business Day Request) Get Technical Data sheet
(Instant Email Delivery) Request Safety Data sheet
(1-2 Business Day Request)
Applications
Certifications
ASTM E595 Compliant
Meets EU Directive 2015/863