Supreme 18TC

Specially formulated one component conductive epoxy adhesive featuring very low thermal resistance properties; meets NASA low outgassing specification
Key Features
  • Can be applied in very thin bond lines
  • High thermal conductivity
  • Unmatched heat transfer capabilities
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
paste
Cure Schedule
90 minutes at 250°F or 60 minutes at 300°F
Hardness
80-90 Shore D
Service Temperature Range
4K to +400°F
Glass Transition Temperature (Tg)
135-140°C
Tensile Lap Shear Strength
2,200-2,400 psi
Image
Supreme 18TC One Part Epoxy Compound
Certifications

ASTM E595 Compliant

1,000 Hours at 85°C/85% RH

Meets EU Directive 2015/863

Packaging
וידאו

Product Spotlight Supreme 18TC

This video demonstrates the ease of use and impressive properties of Master Bond Supreme 18TC, a one component smooth epoxy paste adhesive. Formulated with a blend of special thermally conductive fillers, this system can be applied in bond lines as t …
Product Description

Master Bond Supreme 18TC is a cutting edge material pertaining to the thermal management of epoxies. This system utilizes a special blend of highly thermally conductive filler material that is capable of being applied in bond lines as thin as 10-15 microns. Supreme 18TC maintains high bond strength properties even when exposed to hostile environmental conditions, including elevated temperatures.

Supreme 18TC has very low thermal resistance, since it is highly thermally conductive and able to cure effectively in thin layers. Another way of looking at this is to say that the lower the thermal resistance, the better the heat transfer. In this regard, Master Bond utilizes the principles based on the formula: R=t/K (where “R” is the thermal resistance; “t”, the thickness and “K” the thermal conductivity of the material). Using specific values, when standard alumina filled thermally conductive epoxy is applied in 50 micron thick sections, the thermal resistance is 30-35 x 10-6 K•m2/W. With Supreme 18TC, the thermal resistance is significantly lower: 8-12 x 10-6 K•m2/W, because of the filler and its ability to be effectively applied in sections of 10-15 microns in width. Simply put, this epoxy is second to none when transferring heat.

Significantly, Supreme 18TC is a one part system that requires no mixing. Its working life is essentially unlimited as it is not premixed and frozen. It is has a smooth paste consistency that requires heat curing for 60-90 minutes at 250-300°F with a post cure of a few hours to obtain optimal properties. Some other positives include low shrinkage upon curing, a low CTE and a high degree of dimensional stability. It bonds well to a wide variety of substrates including metals, composites, ceramics and plastics. Supreme 18TC is designed to withstand thermal cycling and shock. Electrically, it is an outstanding insulator. The operating temperature is 4K to +400°F and the color is gray. The forte of Supreme 18TC is high heat transfer and its simple handling, which allows it to be a prime candidate for sophisticated, high-tech applications. Some of the industries where this can be used include aerospace, electronic, optical, specialty OEM and cryogenic industries.

Product Advantages

  • One part system; no mixing required
  • Cures readily at 250-300°F with a post cure at 350°F
  • High thermal conductivity and electrical insulation values
  • Will cure effectively in very thin sections
  • Superior thermal cycling capabilities
  • Exceptionally low thermal resistance
  • Meets NASA low outgassing specifications
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.