Supreme 33ND

Two component, toughened epoxy for bonding and sealing with high temperature resistance
Key Features
  • Easy processing
  • Paste consistency
  • NASA low outgassing
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: paste, Part B: paste
Cure Schedule
75°F: 48-72 hours; 200°F: 2-3 hours
Hardness
75-85 Shore D
Service Temperature Range
4K to +425°F
Coefficient of Thermal Expansion
35-40 x 10⁻⁶ in/in/°C
Glass Transition Temperature (Tg)
115-120°C
תמונה
Supreme 33ND Two Part Epoxy System
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Packaging
Product Description

Master Bond epoxy system Supreme 33ND offers a highly attractive blend of superb physical strength properties, outstanding temperature resistance and easy handling along with a non-drip viscosity. The mix ratio is 100 to 70 by weight or 1 to 1 by volume. This non-flowable system bonds well to many different kinds of substrates including metals, composites, glass, ceramics, rubbers and plastics. t is cryogenically serviceable and has a wide temperature range extending from 4K up to +425°F. It is highly resistant to aggressive thermal cycling. It also has very good chemical resistance to water, fuels, hydraulics as well as many acids and bases. It is a solid electrical insulator with superior retention of those properties at elevated temperatures. Supreme 33ND has a number of curing options including cure schedules at room temperature, with heat or a combination of the two. The optimum cure is overnight at room temperature followed by a few hours at 150-200°F. Part A is colored gray and Part B is amber. Its exceptional dimensional stability and minimal shrinkage upon curing enables it to be an excellent choice for applications in the aerospace, electronic and specialty OEM industries.

Product Advantages

  • Forgiving mix ratios: 100:70 by weight or 1:1 by volume
  • Bonds well to a wide variety of substrates
  • Cryogenically serviceable
  • Passes NASA low outgassing
  • Withstands 1,000 hours 85°C/85% RH
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.