Supreme 3AOHT

One component, fast curing epoxy for bonding, sealing and coating
Key Features
  • One part, no mix epoxy system
  • Thermally conductive, eletrically insulative
  • Fast curing, minimum 250°F
  • Withstands rigorous thermal cycling
    Typical Properties
    Viscosity
    Paste
    Cure Schedule
    250°F for 20-30 minutes; 300°F for 5-10 minutes
    Hardness
    >85 Shore D
    Service Temperature Range
    -100°F to +350°F
    Coefficient of Thermal Expansion
    30-35 x 10⁻⁶ in/in/°C
    Dielectric Constant
    4.1
    Tensile Lap Shear Strength
    >1,600 psi
    Thermal Conductivity
    9-10 BTU•in/(ft²•hr•°F) [1.30-1.44 W/(m•K)]
    Volume Resistivity
    >10¹⁵ ohm-cm
    תמונה
    Supreme 3AOHT One Part Epoxy
    Applications
    Certifications

    Meets EU Directive 2015/863

    Packaging
    Product Description

    Master Bond Supreme 3AOHT combines easy processing, excellent thermal conductivity and electrical insulation properties, along with an enhanced ability to resist thermal cycling. This one part system requires no mixing and can be stored at room temperature or in a refrigerator. It requires oven curing at a minimum temperature of 250°F and will cure more quickly at 300°F. Subsequently, its working life at room temperature is essentially unlimited. It bonds well to a wide variety of substrates including glass, metals, ceramics and most plastics. Additionally, it has superior physical strength properties as well as being a very good electrical insulator. It is also noteworthy for its superb dimensional stability. Supreme 3AOHT is a flexibilized system with good toughness and the ability to withstand thermal cycling and thermal and mechanical shocks. The service temperature range is -100°F to +350°F. It is 100% reactive and does not contain any diluents or solvents. Supreme 3AOHT possesses good chemical resistance to water, oils and fuels. The color of Supreme 3AOHT is off white. This epoxy is widely used in electronic, electrical, aerospace and special OEM applications where a high performance, good thermal conductivity and electrical isolation along with fast curing is desirable.

    Product Advantages

    • Single component system, no mixing required
    • Unlimited working life at room temperature
    • Fast curing, minimum temperature 250°F
    • Superb thermal conductor and electrical insulator
    • Toughened system, resists cycling and shock
    • Outstanding dimensional stability
    Show More

    How to order

    Verify Your Product Selection

    With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

    Get a Quote

    Our customer service team will follow up with a detailed quote with packaging and shipping options.

    Place Your Order

    We'll work with your company to process the order efficiently.

    Receive Your Material

    Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.