Supreme 3HTND-2DA

One component, toughened, electrically insulating epoxy for die attach applications
Key Features
  • Ideal dispensing profile
  • Fast curing
  • High die shear strength
  • Very long working life at room temperature
  • NASA low outgassing
  • Not premixed and frozen
Typical Properties
Viscosity
>300,000 cps
Cure Schedule
5-10 minutes at 150°C
Hardness
>70 Shore D
Service Temperature Range
-100°F to +400°F
Coefficient of Thermal Expansion
25-30 X 10⁻⁶ in/in/°C
Dielectric Constant
4.5
תמונה
Supreme 3HTND-2DA One Part Epoxy
Applications
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

1,000 Hours at 85°C/85% RH

Packaging
Product Description

Master Bond Supreme 3HTND-2DA is a fast curing, one component, high performance, insulating epoxy system for die attach applications. Unlike most other die attach systems, Supreme 3HTND-2DA is not premixed and frozen. It is a true one part system with unlimited working life at room temperature and requiring only simple refrigeration for storage. The system is fast setting with a cure schedule of 5-10 minutes at 150°C.

Supreme 3HTND-2DA dispenses smoothly and easily, without any tailing and is well suited for automatic dispensing equipment. It can be applied to a defined area without running. Upon curing, this epoxy has an impressive array of outstanding properties. First and foremost, it has excellent die shear strength and performed very well in 85/85 testing. It also offers high dimensional stability and a capacity to withstand rigorous thermal cycling and shock. The service temperature range is a robust -100°F to +400°F. Supreme 3HTND-2DA has low ionics, particularly chlorine(<115 ppm). It bonds well to metals, ceramics and silicon dies. It should be noted that while this product is a first class electrical insulator, it has good thermal conductivity. In accordance with die attach requirements, Supreme 3HTND-2DA passes NASA low outgassing test specifications. The extraordinary combination of convenient storage, easy handling and highly desirable properties make this a go-to material not only for die attach applications, but for other bonding situations as well.

Product Advantages

  • Single component system, no mixing needed
  • Unlimited working life at room temperature
  • Desirable dispensing profile, no tailing or bleed out
  • Formidable die shear strength
  • Withstands thermal cycling and shock
  • Excellent dimensional stability
  • Compatible with dispensing equipment
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.