Supreme 62-1

Two component epoxy resin system featuring excellent temperature and chemical resistance
Key Features
  • Convenient handling, long open time
  • Cures rapidly at moderately elevated temperatures
  • Superb physical strength profile
  • Good toughness
Typical Properties
Viscosity
15,000-25,000 cps
Cure Schedule
Typical cure schedules range from 4-6 hours at 140-158°F [60-70°C], 20-40 minutes at 176-212°F [80-100°C] or 10-20 minutes at 257°F [125°C]
Hardness
75-85 Shore D
Service Temperature Range
-60°F to +450°F
Dielectric Constant
4.2
Tensile Lap Shear Strength
1,600-1,800 psi
תמונה
Supreme 62-1 Two Part Epoxy
Product Description

Master Bond Supreme 62-1 is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a very forgiving 100 to 10 mix ratio by weight. The pot life of 100 grams is greater than 12 hours. Typical cure schedules range from 4-6 hours at 140-158°F [60-70°C], 20-40 minutes at 176-212°F [80-100°C] or 10-20 minutes at 257°F [125°C]. To obtain optimum properties, post curing at 212-302°F [100-150°C] for 2-4 hours is recommended. Following an optimum cure schedule, Supreme 62-1 has a glass transition temperature in the range of 120-130°C. Also noteworthy is its outstanding chemical resistance to acids, bases, many solvents and other chemicals, even at elevated temperatures (as listed in the table below). This system has excellent electrical insulation properties. Most noteworthy is that Supreme 62-1 is a toughened system with an enhanced ability to withstand thermal cycling. The service temperature range is -60°F to +450°F The color of Part A is clear and Part B is dark brown in color. Supreme 62-1 is a worthy candidate for aerospace, electronic, optical, specialty OEM and related applications, particularly when high temperature resistance, a degree of toughness and the ability to withstand aggressive chemicals is required.

Product Advantages

  • Easy to use, very forgiving 100 to 10 mix ratio by weight (will fully cure using 100 to 5 mix ratio)
  • Impressively long working life
  • First rate electrical insulation properties
  • Protection from many aggressive chemicals
  • Versatile curing schedules
  • Outstanding dimensional stability
  • Meets NASA low outgassing specifications
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.