UV10TK

One component, moderate viscosity UV curable system for bonding, sealing and encapsulating
Key Features
  • Outstanding optical clarity
  • High glass transition temperature
  • Can cure up to 1/4 inch thick
  • Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
6,000-8,000 cps
Cure Schedule
20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts per cm²
Hardness
>65 Shore D
Coefficient of Thermal Expansion
55-60 in/in X 10⁻⁶°C
Dielectric Constant
3.5
Glass Transition Temperature (Tg)
75-80°C
Refractive Index
1.557
Volume Resistivity
>10¹⁴ ohm-cm
תמונה
Certifications

1,000 Hours at 85°C/85% RH

Meets EU Directive 2015/863

Product Description

Master Bond UV10TK is a moderate viscosity, one part UV system for bonding, sealing and coating with good optical clarity, excellent physical properties and a high glass transition temperature (Tg) of 110-115°C. When exposed to a UV light source emitting at a wavelength of 320-365 nm with 20-40 milliwatts per cm², UV10TK cures readily in 20-30 seconds. The rate of cure depends upon the distance from the light source, the thickness of the section and the intensity of the light source. When bonding, a few thousandths of an inch are more than adequate, and when encapsulating, it can cure in sections up to 1/4 inch thick. It bonds well to glass, surface treated metals and plastics such as polycarbonates and acrylics, among others. Its chemical resistance is particularly good as it resists water, oils, acids, bases and solvents. It is also an effective sealing and coating material. The system does not contain any solvents or diluents and none are released during cure. UV10TK combines low shrinkage with exceptional dimensional stability. It is an outstanding electrical insulator with a temperature range of -60°F to +400°F. UV10TK is effectively used for high production applications where fast fixture times and rapid curing are critical. It is best used in fiber-optic, optical, opto-electronic and electronic industries where high temperature resistance and moderate viscosity are needed.

Product Advantages

  • One component system
  • Moderate viscosity
  • Good temperature and chemical resistance
  • Adheres well to many substrates
  • Outstanding optical clarity; excellent light transmission
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.