UV15X-6NM-2

UV system for high performance bonding, sealing and coating
Key Features
  • Outstanding abrasion resistance
  • Superior non-yellowing properties
  • Excellent flexibility and toughness
  • Moderate viscosity
Typical Properties
Viscosity
35,000-55,000 cps
Cure Schedule
cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm2
Hardness
25-45 Shore D
Service Temperature Range
-80°F to +250°F
Elongation
>100%
Refractive Index
1.50
תמונה
UV15X-6NM-2 One Part UV Curable Epoxy Compound
Certifications

Meets EU Directive 2015/863

Product Description

Master Bond UV15X-6NM-2 is a one component, UV curing urethane acrylate system featuring vibrant flexibility, excellent toughness and superior abrasion resistance. This moderate viscosity compound can be used for a wide variety of applications including bonding, sealing, coating and encapsulation. Its robust flexibility gives it the capacity to withstand severe thermal cycling as well as resisting thermal and mechanical shocks. UV15X-6NM-2 bonds well to a variety of substrates including glass, plastics including polycarbonates and acrylics, composites, metals and many types of rubbers. It has very good chemical resistance, especially to water, cleaning agents and oils. UV15X-6NM-2 is a top notch thermal and electrical insulator with a service temperature range of -80°F to +250°F. It should be noted that it has a substantial non-yellowing profile.

UV15X-6NM-2 generally cures readily in 20-30 seconds when exposed to a UV light source emitting at a wavelength of 320-365 nm with an energy output as low as 20-40 milliwatts/cm². The rate of cure depends upon the system’s distance from the light source, the thickness of the section and the intensity of the light source. It should be noted that the system can cure in sections approaching 1/4 inch thick. However, when bonding, sections of a few thousandths of an inch are more than adequate. Most importantly, UV15X-6NM-2 does not display oxygen inhibition. This system is widely used in fiber-optic, optical, electronic, semiconductor, microelectronic and laser applications.

Product Advantages

  • One part system with no mixing needed
  • Cures very fast upon exposure to 320-365 nm UV light at ambient temperatures
  • No oxygen inhibition
  • Highly reliable thermal and electrical insulator
  • Outstanding flexibility, toughness and abrasion resistance
  • Performs well in withstanding rigorous thermal cycling as well as thermal and mechanical shocks
  • Superb non-yellowing capabilities
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.