Supreme 45HTND-2
Toughened, two component epoxy system for bonding, sealing and coating
Key Features
- Outstanding temperature resistance
- Superior thermal cycling capabilities
- Excellent electrical insulator
- Non-drip application feature
- Very good peel strength
- Exceptionally long working life
Typical Properties
Viscosity
paste
Cure Schedule
250-300°F for 3-4 hours
Hardness
80-90 Shore D
Service Temperature Range
-100°F to +450°F
Dielectric Constant
4.5
Tensile Lap Shear Strength
>2,500 psi