EP42HT-2ND-2
Two component, room temperature curing epoxy compound featuring high temperature resistance
Dielectric Constant
4.4
Glass Transition Temperature (Tg)
150-155°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
Paste 8-12 hours at 75°F followed by 2-4 hours at 175-250°F 80-90 Shore D -60°F to 450°F /it/tds/ep42ht-2nd-2
EP42HT-2ND-2Med Black Two Part Epoxy System
EP42HT-2ND-2Med Black
Two component, high temperature resistant epoxy compound for medical device assembly
Dielectric Constant
4.0
Glass Transition Temperature (Tg)
150-155°C
  • ISO 10993-5 for Cytotoxicity
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Coating
Part A: >1,000,000 cps, Part B: >250,000 cps overnight at 75°F followed by 6-8 hours at 135-165°F or 4-6 hours at 175-185°F 75-85 Shore D -60°F to +450°F /it/tds/ep42ht-2nd-2med-black
EP42HT-3AO Two Part Epoxy
EP42HT-3AO
Two part, room temperature curable epoxy adhesive, sealant, coating and encapsulating system
Acoustical Impedance
5.3 MRayl
Glass Transition Temperature (Tg)
140-150°C
  • RoHS Compliant
  • NASA Low Outgassing
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
  • Potting
40,000-80,000 cps Cure in 3-4 days at 75°F or 2-3 hours at 150-200°F; Recommended curing is overnight at 75°F followed by 2-3 hours at 150-200°F; Optimum cure schedule: Overnight at 75°F, followed by 2-3 hours at 150-200°F 85-95 Shore D 4K to +400°F /it/tds/ep42ht-3ao
EP42HT-4AOMed Black Two Component Epoxy
EP42HT-4AOMed Black
Two part, thermally conductive epoxy for medical device manufacturing
Coefficient of Thermal Expansion
18-21 x 10⁻⁶ in/in/°C
Tensile Modulus
500,000-550,000 psi
  • RoHS Compliant
  • USP Class VI Medical
  • ISO 10993-5 for Cytotoxicity
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
  • Potting
Part A: 50,000-120,000 cps, Part B: 200-1,000 cps overnight at 75°F, followed by 2-3 hours at 150-200°F 85-90 Shore D 4K to +400°F /it/tds/ep42ht-4aomed-black
EP45HT Two Part Epoxy
EP45HT
Two component epoxy system for bonding, sealing, coating and encapsulation
Glass Transition Temperature (Tg)
150-160°C
Volume Resistivity
>10¹⁴ ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
Part A: 60,000-110,000 cps, Part B: 500-2,500 cps 250°F for 3-4 hours or 300°F for 2-3 hours 75-85 Shore D -80°F to +500°F /it/tds/ep45ht
EP45HTMed Two Part Epoxy System
EP45HTMed
Two component, high temperature resistant, medical grade epoxy resists repeated sterilizations
Glass Transition Temperature (Tg)
150-160°C
Volume Resistivity
>10¹⁴ ohm-cm
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Casting
  • Encapsulation
  • Gap Filling
  • Potting
50,000-60,000 cps 250°F for 3-4 hours or 300°F for 2-3 hours 75-85 Shore D -80°F to 500°F /it/tds/ep45htmed
EP45HTND-2 Two Component Epoxy System
EP45HTND-2
Two component epoxy system for high performance bonding, sealing and coating
Dielectric Constant
4.3
Glass Transition Temperature (Tg)
150-160°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
Part A: paste, Part B: paste 3-4 hours at 250°F or 2-3 hours at 300°F 75-85 Shore D -80°F to +500°F /tds/ep45htnd-2
EP46HT Two Part Epoxy
EP46HT
Two component, heat resistant epoxy system for bonding and sealing
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
175°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Encapsulation
  • Gap Filling
3,000-6,000 cps 250-300°F for 3-4 hours >80 Shore D -80°F to +500°F /it/tds/ep46ht
EP46HT-1 Two Part Epoxy Compound
EP46HT-1
Two component epoxy for structural bonding featuring superlative heat resistance; requires oven curing
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
230-240°C
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
15,000-35,000 cps 250-300°F for 2-3 hours, followed by a post cure for optimum properties at 350-400°F for 2 hours 80-90 Shore D -100°F to +600°F /it/tds/ep46ht-1
EP46HT-1ND2 Two Part Epoxy System
EP46HT-1ND-2
Two component epoxy paste for structural bonding featuring superlative heat resistance; requires oven curing. Will not flow during processing
Dielectric Strength
450 volts/mil
Tensile Lap Shear Strength
>2,200 psi
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Coating
paste 250-300°F for 2-3 hours, followed by a post cure for optimum properties at 350-400°F for 2 hours 80-90 Shore D -100°F to +600°F /it/tds/ep46ht-1nd-2