EP46HT
Two component, heat resistant epoxy system for bonding and sealing
Key Features
- Long-term high temperature structural strength retention
- Superior durability, thermal shock resistance
- Exceptional chemical resistance
- Resists up to +500°F
- Low viscosity
- Long pot life
Typical Properties
Viscosity
3,000-6,000 cps
Cure Schedule
250-300°F for 3-4 hours
Hardness
>80 Shore D
Service Temperature Range
-80°F to +500°F
Dielectric Strength
450 volts/mil
Glass Transition Temperature (Tg)
175°C