EP3HT One Part Epoxy
EP3HT
One component epoxy system for bonding, sealing and coating
Dielectric Constant
3.7
Tensile Lap Shear Strength
2,000-2,200 psi
  • RoHS Compliant
  • 1,000 Hours at 85°C/85% RH
  • Bonding
  • Sealing
  • Coating
100,000-200,000 cps 250°F for 20-30 minutes, 300°F for 5-10 minutes 80-90 Shore D -60°F to +400°F /it/tds/ep3ht
EP3HTMed One Part Epoxy
EP3HTMed
One part, heat curing, biocompatible epoxy compound
Tensile Lap Shear Strength
1,600-1,800 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
  • Sealing
  • Coating
100,000-200,000 cps 250°F for 20-30 minutes, 300°F for 5-10 minutes, followed by 1 to 3 hours at +250 to +300°F 80-90 Shore D -60°F to +400°F /it/tds/ep3htmed
EP3HTND-2 Black
One part, heat curing black epoxy compound with paste consistency
Tensile Lap Shear Strength
1,600-1,800 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 250°F for 20-30 minutes, 300°F for 5-10 minutes 80-90 Shore D -60°F to +400°F /it/tds/ep3htnd-2-black
One Part Epoxy EP3HTND-2Med-Black
EP3HTND-2Med Black
One part, heat curing, biocompatible epoxy compound with paste consistency
Tensile Lap Shear Strength
1,600-1,800 psi
Volume Resistivity
>10¹⁴ ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • USP Class VI Medical
  • Bonding
  • Sealing
  • Gap Filling
paste 250°F for 20-30 minutes, 300°F for 5-10 minutes 80-90 Shore D -60°F to +400°F /it/tds/ep3htnd-2med-black
EP3HTS One Part Epoxy
EP3HTS
One part, electrically conductive epoxy system
Tensile Lap Shear Strength
>400 psi
Volume Resistivity
<0.001 ohm-cm
  • RoHS Compliant
  • Bonding
  • Sealing
  • Gap Filling
  • Coating
paste 45-90 minutes at 250°F or 20-40 minutes at 300°F 65 Shore D -60°F to +400°F /it/tds/ep3hts
One Component Epoxy Compound
EP3HTS-LO
One part, high performance, electrically conductive epoxy, NASA low outgassing compliant
Tensile Lap Shear Strength
>400 psi
Volume Resistivity
<0.001 ohm-cm
  • NASA Low Outgassing
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste Cures readily at 250°F at 45-50 minutes or in just 20-30 minutes at 300°F. 65-75 Shore D -60°F to +400°F /it/tds/ep3hts-lo
EP3HTSCN One Part Epoxy
EP3HTSCN
One part, high performance, electrically conductive epoxy
Tensile Lap Shear Strength
900-1,100 psi
Volume Resistivity
0.05 to 0.10 ohm-cm
  • RoHS Compliant
  • Coating
  • Bonding
  • Sealing
  • Gap Filling
paste cures readily at 250°F at 45-50 minutes or in just 20-30 minutes at 300°F 75-85 Shore D -60°F to +400°F /it/tds/ep3htscn
EP3HTSDA-2Med One Part Silver Filled Epoxy
EP3HTSDA-2Med
One component, medical grade, electrically conductive epoxy featuring exceptionally high thermal conductivity
Thermal Conductivity
45-49 BTU•in/(ft²•hr•°F) W/(m•K)]
Volume Resistivity
<0.001 ohm-cm
  • ISO 10993-5 for Cytotoxicity
  • RoHS Compliant
  • Bonding
  • Die Attach
  • Gap Filling
  • Sealing
  • Coating
>400,000 cps 250°F for 20-30 minutes, 300°F for 5-10 minutes 75-85 Shore D -80°F to +450°F /it/tds/ep3htsda-2med
EP3HTSMed One Part Medical Grade Epoxy
EP3HTSMed
One part, electrically conductive, biocompatible epoxy system
Tensile Lap Shear Strength
>400 psi
Volume Resistivity
<0.001 ohm-cm
  • USP Class VI Medical
  • RoHS Compliant
  • Bonding
  • Sealing
  • Coating
  • Gap Filling
paste 40-90 minutes at 250°F or 20-40 minutes at 300°F (minimum cure temperature is 235-240°F) 60-80 Shore D -60°F to +400°F /it/tds/ep3htsmed
EP3RR-80: One Part Epoxy System
EP3RR-80
One component epoxy system for bonding, sealing, potting and encapsulation applications featuring curing temperatures of 175-180°F or higher
Dielectric Constant
4.4
Volume Resistivity
10¹⁴ ohm-cm
  • MIL-STD-810G for Fungus Resistance
  • NASA Low Outgassing
  • 1,000 Hours at 85°C/85% RH
  • RoHS Compliant
  • Sealing
  • Encapsulation
  • Potting
  • Bonding
60,000-120,000 cps Cure in 45-50 minutes at 175-180°F, or in 25-30 minutes 250°F 80-90 Shore D -100°F to +350°F /tds/ep3rr-80