EP21TDCSMed

Silver conductive, two component epoxy for medical applications
Key Features
  • Convenient handling
  • High electrical conductivity
  • Thermally conductive
  • Capable of withstanding thermal cycling
  • Good strength properties
  • USP Class VI certified
Typical Properties
Viscosity
paste
Cure Schedule
overnight at 75°F followed by 2-3 hours at 150-200°F
Hardness
50-60 Shore D
Service Temperature Range
4K to +250°F
Tensile Lap Shear Strength
800-1,000 psi
Volume Resistivity
less than 0.001 ohm-cm
Immagine
EP21TDCSMed Two Part Medical Grade Epoxy
Certifications

Meets EU Directive 2015/863

USP Class VI Medical

ISO 10993-5 for Cytotoxicity

Product Description

Master Bond EP21TDCSMed is a two component, silver filled, electrically conductive epoxy. It can be used for bonding, sealing and coating applications. This system has been tested for USP Class VI specifications for biocompatibility. EP21TDCSMed has a paste consistency and a forgiving one to one mix ratio by weight. It is formulated to cure at room temperature or elevated temperatures with the optimum cure being overnight at room temperature followed by 2-3 hours at 150-200°F.

First and foremost, upon full cure, EP21TDCSMed has superb electrical conductivity with the volume resistivity being less than 10-3 ohm-cm. It bonds well to a wide variety of substrates including metals, composites, glass, ceramics and many plastics. It has reasonably good strength in both shear and peel modes. This system is specially formulated to be more forgiving than most epoxies and is capable of withstanding vigorous thermal cycling. EP21TDCSMed holds up very well to cleaning solutions and sterilants such as EtO and gamma radiation. It is serviceable over the wide temperature range of 4K to +250°F. Parts A and B are both colored silver. EP21TDCSMed is widely used in medical electronic applications where superior conductivity and biocompatibility are important requirements.

Product Advantages

  • Convenient mixing: one to one ratio by weight
  • Contains no volatiles; excellent low outgassing properties
  • Easy application: contact pressure only required for cure; adhesive spreads evenly and smoothly
  • High bond strength to similar and dissimilar substrates
  • Superior durability, thermal shock and chemical resistance
  • Much less rigid than conventional silver epoxy
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.