EP30
Highly versatile, two part epoxy system for bonding, coating, sealing and casting
Key Features
- Superb optical clarity
- Low shrinkage upon curing
- Very low viscosity
- Withstands 1,000 hours 85°C/85% RH
Typical Properties
Viscosity
Part A: 400-900 cps, Part B: 280-500 cps
Cure Schedule
can be cured at 75°F in 24-48 hours or faster cures can be realized at elevated temperatures, e.g., 2-3 hours at 200°F
Hardness
80-90 Shore D
Service Temperature Range
-60°F to +250°F
Dielectric Strength
440 volts/mil
Refractive Index
1.57
Immagine