EP55TCFL

Thermally conductive, electrically isolating epoxy for bonding and sealing; available as a two part system or one part premixed and frozen

Key Features
  • Good flexibility and toughness
  • Flows smoothly and readily
  • Low modulus
  • Meets NASA low outgassing specifications
     
Typical Properties
Viscosity
30,000-60,000 cps
Cure Schedule
50-70°C 4-6 hours; 80-90°C 3-4 hours
Hardness
55-65 Shore D
Service Temperature Range
-50°C to +125°C
Dielectric Constant
4.4
Thermal Conductivity
3.2-3.8 W/(m•K)
Image
EP55TCFL Epoxy System
Certifications

ASTM E595 Compliant

Meets EU Directive 2015/863

Product Description

Master Bond EP55TCFL is available as either a two part or one part system, which will be described in more detail below. Regardless of the packaging, the cured properties are the same. Both are thermally conductive and electrically isolating, and can be used for bonding, sealing and coating. The system has a moderate viscosity that spreads evenly and smoothly when bonding. Curing is also the same, with two cure schedule options: 4-6 hours at 50-70°C or 3-4 hours at 80-90°C. The system has outstanding dimensional stability, no solvents or diluents, and low shrinkage upon curing.

The two part system is packaged in 1, 4, and 8 ounce jars and requires hand mixing with a ratio of 100:15 by weight. It should be stored in a refrigerator at 40–50°F and has a shelf life of 1-3 months. No special shipping conditions are required. The two part system is reusable and should be returned to the refrigerator for storage.

The one part system is premixed and frozen, packaged in syringes of 3 cc, 5 cc, or 10 cc for single use. It must be stored in a cryogenic freezer at –40°C and has a shelf life of 6 months. It is shipped at –40°C with dry ice. Prior to use, the syringe must be removed from the freezer and allowed to reach room temperature. Once thawed, it should not be returned to the freezer. Under no circumstances is the one part system reusable.

EP55TCFL bonds well to a variety of substrates such as metals, composites, ceramics and many plastics. It has good resistance to water, oils and fuels. It is gray in color, and has a service temperature range of -50°C to +125°C. The system is noteworthy for its toughness, low modulus and thermal cycling capabilities. 

It has good flow properties which make it well-suited for small potting and encapsulation applications, where it can be applied in layers up to 1/4 inch thick.
EP55TCFL has a special thermally conductive filler with small particle sizes, which allows it to be applied in very thin bond lines. This results in lower thermal resistance and increases the heat transfer properties of the system. As such, it is a highly effective thermal interface material for bonding applications in microelectronic packaging and assembly. 

Product Advantages

  • High thermal conductivity and electrically insulating
  • Good flexibility, withstands thermal cycling
  • Versatile cure schedules
  • Small particle size lowers thermal resistance
  • NASA low outgassing
Show More

How to order

Verify Your Product Selection

With thousands of custom formulations available, our expert engineers provide personalized consultation to ensure you select the ideal adhesive. We will follow up with a product and packaging recommendation for your specific application.

Get a Quote

Our customer service team will follow up with a detailed quote with packaging and shipping options.

Place Your Order

We'll work with your company to process the order efficiently.

Receive Your Material

Your adhesive will be made to order and shipped to you. Typical lead times are 10-14 business days, with rush options available for urgent orders.