Supreme 11ANHT
Two component epoxy compound for bonding, coating and sealing
Key Features
- Thermally conductive, electrically insulative
- Room temperature curing
- Toughened system, withstands thermal cycling
- Excellent physical strength properties
Typical Properties
Viscosity
Part A: 100,000-300,000 cps, Part B: 150,000-350,000 cps
Cure Schedule
8-12 hours at 75°F, plus 1-2 hours at 150-200°F
Hardness
80-90 Shore D
Service Temperature Range
-112°F to +400°F
Dielectric Constant
4.8
Volume Resistivity
>10¹⁴ ohm-cm