Is there a way to bond or seal substrates for high temperature, high vacuum applications?

This application discusses adhesive solutions for bonding and sealing substrates in high-temperature, high-vacuum environments. It reviews key selection criteria such as low outgassing, thermal cycling resistance, bond strength, electrical and thermal conductivity requirements, and processing considerations to help ensure reliable long-term performance in demanding applications.

Bild
Supreme 10HT

The Application

A customer is working on a device that needs to be used in a high vacuum environment. It will also be subjected to severe thermal cycling. The product requires a structural epoxy that features high shear and peel strengths.

Finding the Answers

  • What are the substrates being used and how are they arranged?
  • What are the operating temperatures and conditions?
  • Can heat be added to cure at about 250°F (125°C)?
  • Would the product need to be electrically conductive or electrically insulating?
  • Would the product need to be thermally conductive for heat dissipation or heat transfer?

The Solution

We recommend the Supreme 10HT line of products

Making certain assumptions about the answers to the above questions, we can recommend the Supreme 10HT line of products. Supreme 10HT is an easy to use, one part heat curing system with fast elevated temperature cures. It provides an unlimited working life at room temperature which increases its appeal from a processing standpoint. The product meets NASA (ASTM E-595) standards for low outgassing and offers high peel as well as shear strengths, along with a wide serviceable temperature range.

Based on the geometry or the set-up, Supreme 10HTND-3 or Supreme 10HTCL may be options to consider. Supreme 10HTND-3 is a thoroughly non-drip formulation, which makes it ideal for use on vertical surfaces or in applications where flow during the cure needs to be restricted. On the other hand, Supreme 10HTCL is a slightly lower viscosity system that offers a good degree of flow properties, which makes it easy to apply using a brush.

An additional option might be Supreme 10HT/S, a silver filled system that offers excellent electrical conductivity. Supreme 10AOHT-LO is also available, and it features exceptional thermally conductivity with excellent electrical insulation properties.

Summary of Products

ProductNASA Low OutgassingViscosityThermal ConductivityElectrical ConductivityFlexibility
Supreme 10HTYesHighNoNoYes
Supreme 10HTND-3NoNon-dripNoNoYes
Supreme 10HTCLNoMediumNoNoYes
Supreme 10HT/SYesNon-dripYesYesYes
Supreme 10AOHT-LOYesHighYesNoYes
Supreme 10HTFLNoHighNoNoYes

Meet Our Tech Expert: Rohit Ramnath

imageRohit Ramnath analyzes application oriented issues and provides product solutions for companies in a variety industries. He graduated from Carnegie Mellon University with a masters degree in chemical engineering.